When evaluating a PPF’s stone-chip resistance, buyers should not rely solely on the “Pass” or “Excellent” ratings listed on test reports. You should focus on verifying the testing standards, sample model, film thickness, test specimen structure, impact conditions, damage rating, and laboratory information. In particular, confirm whether the test evaluates the impact resistance of the PPF film itself or the PPF’s protective effect on the underlying automotive paint finish. Only when the testing methods and sample conditions are clearly defined do the test results hold practical value for procurement decisions.

For PPF importers, distributors, and private-label brands, stone-chip resistance is a critical factor in evaluating the performance of automotive paint protection film.

When comparing different manufacturers, you may receive multiple sets of technical documentation. Some suppliers provide ASTM D3170 test reports, some use Gravelometer testing, and others simply state “Excellent Stone Chip Resistance” in their product Technical Data Sheets (TDS).

While this information may appear similar, it is not necessarily directly comparable.

A comprehensive test report should not only present the test results but also specify the type of sample used, the methodology employed, the conditions under which the impact test was conducted, and how the damage was ultimately evaluated.

From a procurement review perspective, this article will introduce the primary methods for PPF stone-chip resistance testing, the key elements of test reports, and how to use this information to compare products from different manufacturers.

What Is Stone-Chip Resistance Testing for PPF?

Stone-Chip Resistance Testing is a method used to evaluate a coating or protective system’s ability to resist damage from stone chips by simulating the impact of gravel or other particles on a vehicle’s surface.

When a vehicle is traveling at high speeds, tires may fling small stones and debris from the road onto the vehicle’s body. Areas such as the front bumper, hood, fenders, and side skirts are more susceptible to such impacts.

The role of PPF is to provide additional protection for the original factory paint finish through a transparent protective film.

However, purchasers need to distinguish between two concepts:

  • Film Damage Resistance: The ability of the PPF film itself to resist impact damage.
  • Paint Protection Performance: The effectiveness of the protection provided to the underlying automotive paint finish after PPF installation.

These two metrics are related but cannot be directly equated.

For example, the presence of some impact marks on the PPF surface after testing does not necessarily mean that the underlying automotive paint has been damaged. Conversely, merely observing that the PPF surface shows no obvious damage does not prove its protective effectiveness without inspecting the underlying paint.

Therefore, buyers should first confirm the test objectives before determining whether the report results meet their procurement requirements.

Which Standards Are Used for PPF Stone-Chip Testing?

There are several common standard methods for stone-chip resistance testing of automotive coatings. Purchasers need to understand the test subjects and evaluation methods of these standards to avoid directly comparing results from different standards.

ASTM D3170: Gravelometer Chip Resistance Test

ASTM D3170/D3170M is a test method used to determine a coating’s ability to resist impact damage from stones or other projectiles.

This method uses a Gravelometer to subject test panels to controlled impacts using specified impact media and equipment conditions, thereby evaluating the coating’s resistance to stone chips.

The main testing procedure includes:

  1. Prepare coating test panels that meet the test requirements.
  2. Prepare and condition the test specimens according to specified conditions.
  3. Mount the test panels in the Gravelometer.
  4. Perform the impact test using the specified impact medium.
  5. Remove loose debris from the test panel surface in accordance with the test method.
  6. Evaluate stone-impact damage according to the applicable rating method.

The test report should clearly specify the test panel configuration, test method, impact conditions, and final rating.

For PPF purchasers, please note: The scope of ASTM D3170 is the stone-impact resistance test for coatings; it is not a standalone certification standard specifically developed for all PPF products.

If a manufacturer applies this method to composite specimens with PPF installed, the specimen configuration and any modifications made to the standard method should be clearly stated.

SAE J400: Test for Chip Resistance of Surface Coatings

SAE J400 is another method used for testing the chip resistance of automotive surface coatings.

It evaluates the chip resistance of a coating system by simulating the impact of gravel on the surface of an automotive coating.

When reviewing SAE J400 reports, purchasers should verify:

  • The version of the standard used.
  • The test equipment and impact medium.
  • The substrate and coating structure of the test specimen.
  • The test conditions.
  • The stone-impact damage rating.
  • The specific failure locations.

SAE J400 is primarily intended for organic surface coating systems on flat test panels. When extending its application to other materials or PPF composite structures, the scope of application and limitations of the test method must be specified.

Do not assume that two reports labeled SAE J400 test exactly the same product structure.

ISO 20567-1: Multi-Impact Stone-Chip Testing

ISO 20567-1:2017 is an important international standard for testing the resistance of automotive coatings to stone chips.

This standard specifies three test methods using chilled-iron grit to impact the surface of test specimens, simulating multiple impacts from small stones on automotive coatings.

Compared to Gravelometer-based tests, this method employs different impact media and test procedures.

During the audit, attention should be paid to:

  • Test Method
  • Abrasive Material
  • Test Panel
  • Specimen Preparation
  • Impact Conditions
  • Test Temperature
  • Damage Evaluation

It is particularly important to note that the multiple-impact method in ISO 20567-1 is not directly interchangeable with the test procedures in ASTM D3170 or SAE J400.

If two manufacturers use different methods, the purchaser should first confirm whether the test conditions are comparable, rather than directly judging product quality based on the report ratings.

Comparison of Common Stone-Chip Test Standards

Test StandardMain ApplicationWhat Buyers Should Verify
ASTM D3170/D3170MCoating chip resistanceGravelometer conditions and damage rating
SAE J400Automotive surface coating chip resistanceTest procedure and rating method
ISO 20567-1Multi-impact coating resistanceChilled-iron grit and impact conditions

These standards primarily address coatings or automotive surface treatment systems. For PPF, manufacturers should clearly specify whether the test specimens include the actual PPF structure and whether the tests have been appropriately adapted.

Does the Test Evaluate PPF Film Damage or Paint Protection?

This is the issue most commonly overlooked when reviewing a PPF Stone-Chip Test Report.

Buyers must know exactly what the test is evaluating.

PPF Film Damage Resistance

The first test objective is to observe the condition of the PPF film itself after being struck by a stone.

Key inspection items include:

  • Film Puncture: Whether the film has been penetrated.
  • Film Tearing: Whether the film has torn.
  • Surface Damage: Whether visible damage is present on the surface.
  • Coating Damage: Whether the surface coating has been damaged.
  • Delamination: Whether separation has occurred between film layers.

For Gloss PPF, attention should also be paid to whether noticeable surface deformation or changes in optical appearance occur after impact.

For Matte, Satin, and Colored PPF, consideration should also be given to whether the surface texture and color are affected.

Underlying Automotive Paint Protection

The second test objective is to evaluate whether the PPF, once installed, can protect the underlying automotive paint under specific stone-impact conditions.

If the purchaser wishes to verify this, they may require the manufacturer to use a clearly defined composite test specimen protocol.

For example:

  1. Prepare representative automotive paint and clear coat test panels.
  2. Install the PPF according to the agreed-upon application method.
  3. Record the film model, thickness, and installation conditions.
  4. Conduct the stone-impact test using the method agreed upon by both parties.
  5. Inspect the PPF for penetration, tearing, or delamination.
  6. Remove the PPF under specified conditions.
  7. Inspect the underlying clear coat and paint for damage.

It is important to note that if adjustments are made to the standard test specimens or procedures for this composite structure test, they should be accurately documented as an applicable modified test protocol; the test should not be directly claimed to fully comply with all requirements of the original standard.

For brand owners seeking to procure high-performance PPF, it is recommended to prioritize test evidence demonstrating the protective effectiveness of the underlying paint surface, rather than focusing solely on the impact results of the film’s surface.

What Should Buyers Verify in a PPF Stone-Chip Test Report?

Upon receiving a test report from the manufacturer, it is recommended to review it based on the following eight criteria.

1. Test Standard and Method

First, confirm the standard and specific test method used in the report.

Check:

  • ASTM D3170/D3170M
  • SAE J400
  • ISO 20567-1
  • Manufacturer-Specific Test Method

Also verify the standard version, test procedures, and whether there are any deviations from the method.

If the report only states “ASTM D3170” without further details on the sample configuration and test conditions, the manufacturer should be asked to provide additional information.

2. Sample Identification and Film Thickness

Confirm that the test samples match the actual purchased products.

Verification ItemRequired Information
Product NamePPF Product Name
Product ModelSpecific Product Model
TPU MaterialTPU Material Specifications
Film ThicknessNominal Thickness and Measurement Caliber
Film ConstructionFilm Layer Structure
Top CoatSurface Coating Information
AdhesiveAdhesive Specifications
Sample BatchSample Batch
Test DateTest Date

Pay special attention to Film Thickness.

If the report tests one thickness, but the purchaser actually buys a different thickness, the report cannot be directly used as complete proof of the current product’s performance.

Additionally, PPF performance is also influenced by the type of TPU, coatings, adhesive layer, and overall structure.

Therefore, stone-chip resistance cannot be judged based solely on thickness figures.

3. Substrate and Film Application

This is a critical factor in determining whether the report has practical value for procurement.

Items to verify:

  • Was a metal panel or another substrate used?
  • Was an automotive paint test panel used?
  • Does it include a clear coat?
  • Was the PPF installed on the test panel?
  • What installation method was used?
  • Is the post-installation curing time recorded?
  • Does the film structure match that of the actual product?

If the report only states “Painted Metal Panel” without specifying whether PPF was installed, it is impossible to determine whether the test evaluated a standard coating or a PPF composite structure.

If the test objective is to protect the underlying paint surface, a complete description of the test specimen’s structure should be requested.

4. Test Conditions and Impact Parameters

Test conditions directly affect the final results.

It is recommended to verify the following information:

Test ParameterWhat Buyers Should Verify
Test EquipmentGravelometer model and equipment condition
Impact MediaImpact media type
Media SpecificationMedia size, grade, or specifications
Air PressureApplicable impact pressure
Impact AngleApplicable impact angle
Exposure TimeImpact duration or media projection conditions
Test TemperatureTest Temperature
Number of CyclesNumber of Impact Cycles
Specimen ConditioningSpecimen Conditioning Conditions

Different test methods do not necessarily use exactly the same parameters.

Therefore, you should verify, based on the declared standard and specific test procedure, whether the report records the applicable parameters and any deviations.

Pay particular attention to the test temperature. Temperature can affect the toughness of polymer materials and the performance of coatings.

If two reports use different test temperatures, the results should not be directly considered as a comparison under equivalent conditions.

5. Test Results and Damage Evaluation

Test results should not be evaluated solely as “Pass” or “Fail.”

The report should be required to specify the specific evaluation methods used.

Key areas of focus:

  • Chipping Rating
  • Number of Chips
  • Chip Size Distribution
  • Damaged Area
  • Film Puncture
  • Film Tearing
  • Delamination
  • Underlying Paint Damage

Different standards may use different rating systems.

For example, ratings under ASTM D3170 use a combination of letters and numbers to indicate the number of chips in different size categories.

Buyers should confirm the rating rules used in the report and ask the manufacturer to explain the specific damage conditions represented by each rating.

If the report only states:

Stone-Chip Resistance: Pass

without test conditions, specific results, or photos of the damage, it provides only limited reference information.

6. Test Photos and Visual Evidence

Photos are important supporting materials for verifying the test process and results.

It is recommended to request the following from the manufacturer:

  • Before-Test Photos
  • After-Test Photos
  • Close-Up Damage Photos
  • PPF Removal Photos (if applicable)
  • Underlying Paint Inspection Photos (if applicable)

The photos should correspond to the report number, sample number, and test date.

If the report claims that there is no visible damage to the underlying automotive paint, photos of the underlying paint inspection after PPF removal should be provided whenever possible.

7. Laboratory Information and Accreditation

If the report is issued by a third-party laboratory, the following must be verified:

  • Laboratory Name
  • Report Number
  • Testing Date
  • Sample Identification
  • Test Method
  • Authorized Signature
  • Accreditation Information

For ISO/IEC 17025-accredited laboratories, you should also verify whether the relevant test items fall within the scope of their accreditation.

The fact that a laboratory holds ISO/IEC 17025 accreditation does not mean that all of its test items are automatically accredited.

If the report is issued by the manufacturer’s in-house laboratory, it is also necessary to understand the equipment, testing methods, personnel capabilities, and record-keeping practices.

In-house test reports can serve as a reference for the supplier’s quality management but cannot automatically be equated with independent third-party test reports.

8. Conclusion and Test Limitations

Finally, verify that the report’s conclusion aligns with the actual test results.

Common phrasings include:

  • Pass
  • Fail
  • No Significant Damage Observed
  • No Detrimental Effect
  • Within Agreed Acceptance Criteria

These phrasings should not be simply interpreted as indicating the complete absence of any damage.

For example, “No Detrimental Effect” may indicate that no harmful changes meeting the specified criteria were detected; it does not necessarily mean the test specimen was completely unaffected by impact.

Purchasers should request that manufacturers explain the basis for the final conclusion, as well as the products and test conditions to which the report applies.

How to Compare Stone-Chip Test Reports from Different PPF Manufacturers

When you receive test reports from multiple suppliers, it is not recommended to compare only the final ratings.

The correct approach is to first confirm whether the test conditions are comparable.

For example, suppose you are comparing two Gloss TPU PPF products:

Verification ItemSupplier ASupplier B
Test StandardASTM D3170SAE J400
Product TypeGloss TPU PPFGloss TPU PPF
Film Thickness8 mil8 mil
SubstratePainted PanelPainted Panel
Film ApplicationNot SpecifiedInstalled PPF
Test TemperatureAmbientLow Temperature
Test ResultPassRating Provided
Test PhotosNot ProvidedProvided

As shown in the table, although both reports cover stone-impact resistance testing, the sample structures and test conditions are not entirely consistent.

At this point, it cannot be simply concluded that Supplier A’s or Supplier B’s product is superior.

The purchaser should first request that both parties provide more comprehensive test data.

To ensure a fair comparison, it is recommended to standardize the following as much as possible:

  1. Test Standard and Edition.
  2. Product Model and Film Construction.
  3. Film Thickness and Measurement Method.
  4. Substrate and Clear Coat.
  5. PPF Installation Procedure.
  6. Impact Conditions.
  7. Damage Evaluation Method.
  8. Number of Test Specimens.

If the test standards cannot be standardized, it is at least necessary to clarify the differences and scope of application between the two test methods.

For high-value OEM projects, consider commissioning a third-party laboratory with the appropriate testing capabilities to conduct comparative testing according to a standardized protocol agreed upon by both parties.

Common Mistakes When Evaluating PPF Stone-Chip Test Reports

Purchasers often make the following mistakes when reviewing stone-chip resistance reports.

Mistake 1: Treating “Pass” as a Guarantee of No Damage

“Pass” indicates that the sample meets the relevant criteria under specific test conditions.

It does not imply that the PPF will remain undamaged under all road, speed, temperature, and impact conditions.

Mistake 2: Directly Comparing Different Test Standards

The test procedures and evaluation systems of ASTM D3170, SAE J400, and ISO 20567-1 differ.

Ratings under different standards cannot be simply compared numerically.

Mistake 3: Ignoring the Test Sample Structure

Without knowing whether the test involved a bare coating, a standalone PPF, or a composite PPF structure installed on a vehicle’s paint surface, it is impossible to accurately interpret the report’s conclusions.

Mistake 4: Assuming Thicker PPF Always Performs Better

Film thickness is an important technical parameter, but it is not the sole factor determining stone-chip resistance.

The properties of the TPU material, as well as the coating, adhesive layer, and overall structure, also influence product performance.

Mistake 5: Accepting Reports Without Product Identification

If a report does not clearly specify the product model, thickness, and sample information, you cannot confirm whether it applies to the PPF you are currently purchasing.

Mistake 6: Treating Laboratory Accreditation as Universal Approval

ISO/IEC 17025 accreditation must be evaluated in conjunction with the specific scope of accreditation.

One cannot assume that all test results fall within the scope of accreditation simply because the laboratory holds an accreditation certificate.

PPF Stone-Chip Test Report Verification Checklist

It is recommended to use the checklist below before approving a supplier’s PPF technical documentation.

Inspection ItemWhat to VerifyStatus
Test StandardASTM / SAE / ISO / Internal MethodPass / Pending
Standard EditionCorrect version identifiedPass / Pending
Product ModelMatches purchased productPass / Pending
TPU SpecificationConfirmedPass / Pending
Film ThicknessMatches approved specificationPass / Pending
Film ConstructionClearly identifiedPass / Pending
Test SubstrateClearly describedPass / Pending
PPF ApplicationInstallation procedure documentedPass / Pending
Impact MediaType and specification recordedPass / Pending
Test ConditionsApplicable parameters documentedPass / Pending
Test TemperatureRecordedPass / Pending
Damage RatingEvaluation method identifiedPass / Pending
Film DamageResults documentedPass / Pending
Paint ProtectionVerified if requiredPass / Pending
Test PhotosBefore and after evidence availablePass / Pending
LaboratoryIdentity and capability verifiedPass / Pending
Report NumberTraceablePass / Pending
Sample DateRecordedPass / Pending

Final Review Decision:

  • Accepted for Technical Evaluation
  • Additional Information Required
  • Additional Testing Required
  • Not Suitable for Direct Comparison

This checklist is suitable for initial supplier screening, technical documentation review, and the OEM product development phase.

If key parameters are missing from the report, it does not necessarily mean the product is substandard; rather, it indicates that the purchaser has not yet obtained sufficient evidence to confirm its stone-impact resistance.

How FUNOPPF Supports PPF Product Quality Verification

For PPF importers and private-label brands, product development cannot focus solely on price and appearance; it is also essential to verify that product performance aligns with the target market’s positioning.

FUNOPPF offers international customers a wide range of PPF product options, including:

  • Gloss PPF
  • Matte PPF
  • Satin PPF
  • Colored PPF

During product selection and OEM collaboration, we recommend first confirming the following technical requirements:

Product Specification: Clearly define requirements for TPU material, film structure, thickness, surface coating, and adhesive layer.

Sample Evaluation: Evaluate the optical performance, surface quality, installation performance, and related properties of samples prior to mass production.

Performance Verification: Confirm applicable test methods, sample structures, and test data based on the performance requirements of the target product.

Quality Documentation: Confirm the TDS, test reports, and relevant batch quality records based on order requirements.

OEM Customization: Discuss product models, packaging design, labeling, and product line planning based on brand positioning.

For customers seeking to establish a long-term brand and stable procurement channels, we recommend confirming product specifications and key performance indicators before placing a formal order, and incorporating mutually agreed-upon technical requirements into the procurement documentation.

If you are comparing different PPF manufacturers or planning to develop your own PPF brand, you can learn more from our PPF sample testing guide and PPF factory audit guide.

We can discuss suitable PPF product solutions and quality verification requirements based on your target products, procurement specifications, and market demands.

FAQ

Is ASTM D3170 Specifically Designed for PPF?

No. ASTM D3170/D3170M is a test method for evaluating the resistance of coatings to chipping caused by stones or other flying objects. It is not a dedicated certification standard for all PPF products. When applied to PPF, the manufacturer should clearly identify the test specimen structure and any modifications to the standard procedure.

Does Passing ASTM D3170 Mean PPF Will Not Be Damaged by Stones?

No. Passing a test means the specimen met the applicable acceptance criteria under specified conditions. It does not guarantee that the film will never be punctured, torn, or damaged during actual vehicle use.

Can Buyers Compare ASTM D3170 and ISO 20567-1 Results Directly?

No. The two methods use different test procedures, impact media, and evaluation systems. Buyers should compare test conditions and specimen structures before drawing conclusions about relative performance.

Does Thicker PPF Always Provide Better Stone-Chip Protection?

No. Thickness is only one factor. TPU material characteristics, film construction, coating properties, and adhesive performance can also influence impact behavior. Buyers should evaluate the complete product structure rather than relying on thickness alone.

Should PPF Be Tested on Automotive Paint Panels?

If the objective is to evaluate paint protection, testing a representative PPF and automotive paint panel assembly can provide more relevant evidence than examining the film alone. The test setup and any deviations from the original coating test method should be clearly documented.

Can a Stone-Chip Test Report Be Used for Different PPF Models?

Not automatically. The report should identify the tested product, thickness, construction, and sample information. If another PPF model has a different material structure or specification, additional verification may be necessary.

Conclusion

Stone-chip resistance is an important performance consideration when evaluating PPF products for wholesale purchasing and private label development.

However, a test report is only useful when its testing method, sample structure, impact conditions, and evaluation criteria are clearly documented.

Before comparing PPF manufacturers, verify whether the test evaluates the film itself or its protection of the underlying automotive paint. Check the product identification, thickness, substrate, testing conditions, damage rating, and laboratory information.

Most importantly, do not treat a simple “Pass” statement as proof of universal stone-chip protection.

For importers, distributors, and brand owners, a comprehensive technical report provides a stronger basis for supplier evaluation, product positioning, and long-term purchasing decisions.

Looking for PPF products for your wholesale or private label business?

FUNOPPF supplies Gloss PPF, Matte PPF, Satin PPF, and Colored PPF to international distributors, importers, and automotive film brands.

Contact our team to discuss your target product specifications, technical documentation requirements, and OEM cooperation plans.

Table of Contents

Who We Are

FUNO is a Chinese manufacturer of paint protection film and automotive window film.

Talk to FUNO for wholesale supply, private label service, and sample evaluation.

Contact us

Related Posts

Contact FUNO

Tell us your target market, product category, preferred specification, estimated purchasing volume, and whether you need standard or private label supply.

FUNO can help you narrow suitable film options, sample requirements, packaging needs, and the next step toward bulk purchasing.